LeadChem Technical enquiry

Application guide

Folding carton gluing

A glue flap can meet bare board, varnish or film. Identify both faces of the joint before choosing an adhesive for the folder-gluer.

Discuss this application
Kraft-coloured folding carton beside two soap bars
Packaging application example

What does the glue actually touch?

M-6140 and M-6145 are folder-gluer candidates for UV-coated, laminated and varnished carton joints. Their stated viscosity is 7,000–14,000 mPa·s, but the actual glue-contact surfaces determine the trial. Open the seam, mark where each flap touches the adhesive, and compare printed coating with any exposed-board strip before choosing a model.

Which conditions belong in the trial record?

Record both bonding surfaces, nozzle or disc geometry, bead position, line speed and compression time. The folder-gluer family has a source-stated benchmark up to 420 m/min and a 48-hour cure reference. Those figures do not diagnose pop-open: preserve failed seams and distinguish an early opening from separation after conditioning.

The bonding surfaces
Name the board, film or varnish on each side of the joint. Mark any glue-free strip or abraded area.
The folder-gluer setup
Record the nozzle or wheel, bead position, running speed and time under compression.
The failed seam
Show whether the seam springs open at delivery or separates after packing. Note which surface carries the adhesive after opening.

How should the trial be compared with current production?

Compare M-6140 or M-6145 with the current adhesive on the same blank batch and controlled setup. Agree the 24-hour ambient inspection and the separate 48-hour cure reference, then document seam opening and fiber tear. Use the listed thermal exposures only after confirming the test construction and evaluation method with the manufacturing partner.

Why glued cartons pop open →

All applications