Paper packaging adhesives
Compare cold glues for folder gluers and rigid boxes, carton flap sealing adhesives, and film-to-paper lamination adhesives. The bond surfaces, application method and conditioning test determine the trial; model number alone does not.
Compare 18 grades
Which cold-glue family matches folder gluing, rigid boxes or carton sealing?
Start with the application operation. The M-6140–M-6288 folder-gluer group states up to 420 m/min, while the six rigid-box grades beginning with M-6123 share 55±2% solids and fiber tear ≥95%. M-6050/M-6060/M-6070 cover carton sealing; M-7273/M-7285/M-7298 cover film-to-paper lamination. Validate the exact surfaces and feeding system before selecting a grade.
Folder-gluer cold glue
The folder-gluer range has 42±2%, 45±2% and 50±2% solids variants with the same supplied 7000–14000 mPa·s viscosity range. UV-coated, laminated and metallized cartons need actual-stock trials. Speed up to 420 m/min is a source benchmark, not an automatic line capability.
Automatic rigid boxes
The six M-6123/M-6192/M-6296/M-6298/M-6318/M-6328 grades share 55±2% solids, 800–5000 mPa·s viscosity and ≥95% fiber tear. Confirm whether the line uses a diaphragm pump or hopper, the wrap and board construction, assembly pressure and conditioning before grade selection.
Carton flap sealing or film lamination
M-6050/M-6060/M-6070 cover manual or automatic side/bottom sealing, including evaluation of UV/varnished flaps. M-7273/M-7285/M-7298 cover gloss/matte PP/BOPP film to paper. The 12000–25000 versus 100–500 mPa·s ranges belong to different operations and must not be used as interchangeable options.
How do solids and viscosity vary across the 18 adhesive grades?
Compare solids within the intended application family first. M-6140/M-6268 state 42±2%, M-6145/M-6278 state 45±2%, and M-6150/M-6288 state 50±2%; no further distinction between each matching pair is supplied. The six rigid-box grades share 55±2%. Published ranges guide screening but do not establish interchangeability, substrate allocation or a guaranteed coat-weight reduction.
| Grade | Solids | Viscosity | Key test benchmark | Target substrates | Application method |
|---|---|---|---|---|---|
| M-6140 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 42±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6145 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 45±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6150 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 50±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6268 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 42±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6278 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 45±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6288 High-Speed Folder-Gluer Adhesive / Cold GlueRequest TDS / sample | 50±2% | 7000–14000 mPa·s | Up to 420 m/min; 48 h cure; application trial required | UV-coated, gloss/matte laminated, aqueous-varnished and metallized cartons; APET/PVC windows | Straight-line or special-shaped folder gluing; window patching |
| M-6123 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6192 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6296 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6298 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6318 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6328 High-Speed Automatic Box-Making Adhesive / Rigid Box Cold GlueRequest TDS / sample | 55±2% | 800–5000 mPa·s | Fiber tear ≥95%; 48 h cure | Laminated stock, gold/silver board, soft-touch film, aqueous varnish, specialty paper | Automatic rigid-box assembly; diaphragm pump or hopper |
| M-6050 Water-Based Carton Sealing / Polished-Surface AdhesiveRequest TDS / sample | 35±2% | 12000–25000 mPa·s | 48 h cure; finished bond test to be agreed | Color, wine, shoe, pharmaceutical and food cartons; validate UV/varnished glue flaps | Manual or automatic carton side/bottom sealing |
| M-6060 Water-Based Carton Sealing / Polished-Surface AdhesiveRequest TDS / sample | 40±2% | 12000–25000 mPa·s | 48 h cure; finished bond test to be agreed | Color, wine, shoe, pharmaceutical and food cartons; validate UV/varnished glue flaps | Manual or automatic carton side/bottom sealing |
| M-6070 Water-Based Carton Sealing / Polished-Surface AdhesiveRequest TDS / sample | 50±2% | 12000–25000 mPa·s | 48 h cure; finished bond test to be agreed | Color, wine, shoe, pharmaceutical and food cartons; validate UV/varnished glue flaps | Manual or automatic carton side/bottom sealing |
| M-7273 Water-Based Film-to-Paper Lamination AdhesiveRequest TDS / sample | 36±2% | 100–500 mPa·s | 48 h cure; peel target to be agreed | Gloss/matte film and PP/BOPP film to printed paper | Film-to-paper lamination |
| M-7285 Water-Based Film-to-Paper Lamination AdhesiveRequest TDS / sample | 40±2% | 100–500 mPa·s | 48 h cure; peel target to be agreed | Gloss/matte film and PP/BOPP film to printed paper | Film-to-paper lamination |
| M-7298 Water-Based Film-to-Paper Lamination AdhesiveRequest TDS / sample | 44±2% | 100–500 mPa·s | 48 h cure; peel target to be agreed | Gloss/matte film and PP/BOPP film to printed paper | Film-to-paper lamination |
At equal wet adhesive mass, a higher solids fraction leaves more dry material. Substrate absorption, wetting, drying, application weight and pressure still govern the joint, so a higher number does not automatically mean a better bond. All four families state 48 h cure; do not confuse that with the separate 24 h ambient QC conditioning. Approximately 30% lower consumption is source-stated for the folder-gluer group, but no comparator or coat-weight basis was supplied; no saving is predicted here.
Read grade-specific data and method limits
- M-6140: Non-slinging and clean running are source-stated characteristics. Approx. 30% lower consumption is source-stated without a comparator or coat-weight basis, so it is not a predicted saving. Grades with matching figures require technical selection; no unique application split is supplied.
- M-6123: For food, phone, cosmetic, tobacco, wine and jewelry rigid boxes. Matching published ranges do not establish grade interchangeability; confirm the grade on actual stock and feeding equipment.
- M-6050: For carton flap sealing on UV/varnished surfaces, trial the exact finish before confirming the grade.
- M-7273: Low VOC, easy cleanup and fast tack are stated characteristics; no numerical VOC limit or tack test is supplied.
What should be checked for glue slinging, nozzle clogging or carton pop-open?
For M-6140–M-6288 slinging, record application speed, viscosity method and glue delivery before altering settings. For rigid-box pop-open, inspect the bond surfaces and compare conditioning with the stated −36°C and 80°C benchmarks. Nozzle buildup also needs a defined cleanability test. The table lists possible causes and candidate families, not confirmed diagnoses.
| Production defect | Possible root cause | Recommended grade & process checks |
|---|---|---|
| Glue slinging on the folder gluer | Delivery volume, disc condition/speed, viscosity, contamination or material mismatch may contribute. | Screen the M-6140–M-6288 folder-gluer family. Use the 10 min disc protocol and progressively validate the intended line speed up to the stated 420 m/min benchmark; confirm settings with the equipment and adhesive teams. |
| Nozzle clogging or frequent wiping | Dried buildup, contamination, nozzle condition, temperature or an unsuitable feeding system may contribute. | Confirm the chosen grade and spray compatibility before testing. Use 10 kg continuous spraying, average wipe interval ≥30 min and cleaned residue area ≤20% as the supplied QC benchmark, not a guaranteed result for every grade. |
| Cold-chain or ocean-freight pop-open | Poor wetting, short pressure time, incomplete cure, stress or moisture/temperature exposure may contribute. | For folder-gluer grades, compare −20°C/24 h and 60°C/24 h at 85% RH; for rigid-box grades, compare −36°C/24 h and 80°C/48 h at 95% RH. Reproduce the actual joint and shipping exposure; chamber results are not freight guarantees. |
| Rigid-box edge lifting on soft-touch wrap | Low-wetting finish, wrap stress, inconsistent contact or insufficient pressure/cure may contribute. | Screen the six rigid-box grades beginning with M-6123 on the actual soft-touch stock. Confirm pump/hopper feeding, contact and pressure; assess the stated ≥95% fiber-tear benchmark using an agreed procedure. |
| Carton flap seal opens on UV or varnished stock | Finish at the glue flap, contamination, gap or insufficient contact may limit the bond. | Screen M-6050/M-6060/M-6070 for the specified manual/automatic sealing line, or the folder-gluer family for its own application. Test actual UV/varnished flaps; the term polished-surface adhesive is not proof of universal finish compatibility. |
| Film-to-paper lamination delaminates | Film treatment, adhesive transfer, drying, nip conditions or cure may differ from the validated structure. | Screen M-7273/M-7285/M-7298 for PP/BOPP film-to-paper lamination. Identify the failure interface and compare after the stated 48 h cure and agreed conditioning; no numerical peel target is supplied for this group. |
Which substrate and QC records should accompany an adhesive sample request?
Supply both bonding surfaces, the machine and running speed, the target bond test, and packaging or documentation needs. An M-6140 folder-gluer request targeting 420 m/min should describe the coated flap; a rigid-box request for M-6123 should describe wrap, board and feeding. Use the substrate pages and QC protocol to define the trial record before production.
What should converters confirm before changing a cold-glue grade?
Confirm the substrate, delivery system, viscosity method and acceptance test before substituting models. M-6140 and M-6268 share 42±2% solids, while the six rigid-box grades share 55±2%; identical published ranges do not establish interchangeability. The questions below separate useful source benchmarks from performance that must be demonstrated on the converter's own line.
Which cold glues should be screened on a 420 m/min folder gluer?
M-6140, M-6145, M-6150, M-6268, M-6278 and M-6288 form the folder-gluer group, with 7000–14000 mPa·s viscosity and a stated speed up to 420 m/min. Confirm the application system, glue film, pressure and carton finish. The speed figure is a trial reference, not a guarantee for every line.
Does higher solids automatically mean better adhesion or less glue?
The folder-gluer group provides 42±2%, 45±2% and 50±2% solids options. At equal wet application mass, higher solids leaves more dry material, but absorption, wetting, drying and pressure also affect the joint. No model-specific coat weight or substrate allocation is supplied; compare actual joints before claiming savings or substitution.
Which tests apply to folder-gluer and rigid-box cold glues?
Folder-gluer benchmarks are −20°C for 24 h and 60°C for 24 h at 85% RH. The rigid-box group, including M-6123, states −36°C for 24 h and 80°C for 48 h at 95% RH. Confirm conditioning and bond acceptance; these chamber conditions do not predict every freight exposure.
Can the rigid-box grades be treated as interchangeable?
M-6123, M-6192, M-6296, M-6298, M-6318 and M-6328 share supplied ranges of 55±2% solids, 800–5000 mPa·s viscosity, 48 h cure and fiber tear ≥95%. No unique grade-to-stock mapping is provided. Use the actual wrap, board and pump or hopper setup to validate selection and changeovers.
Which grades cover carton flap sealing and BOPP-to-paper lamination?
M-6050, M-6060 and M-6070 cover carton side/bottom sealing at 12000–25000 mPa·s, with the actual UV or varnished flap checked in a trial. M-7273, M-7285 and M-7298 cover gloss/matte PP/BOPP-film-to-paper lamination at 100–500 mPa·s. Both groups state 48 h cure; they serve different application operations.
How is spray-gun cleanability evaluated before a machine trial?
The supplied protocol uses 10 kg of continuous spraying, an average nozzle-wipe interval of at least 30 min and cleaned residue area no greater than 20%. Apply an agreed protocol to the selected grade, such as M-6123, on compatible equipment; this benchmark is not evidence that every listed grade passed.
Typical/source-stated values support initial screening. They are not certifications or warranties. Confirm the latest TDS/SDS, test methods and the complete substrate/process trial before production. Packaging options: 20 kg pail, 50 kg drum and 1000 kg IBC tote.