Coatings for metallized & holographic board

Separate the decorative face, protective layer and adhesive interface. A primer for a metallized card, a coating for aluminum foil and an adhesive touching a metallized film perform different jobs in the finished construction.

Which grades match the metallic face or lamination interface?

LK1024 is the water-based primer candidate for metallized and holographic card, with 30±1% solids and a stated viscosity of 20±2 seconds. LK1025 addresses aluminum foil; LK1026 addresses metallized-film lamination. Select by the layer being coated or bonded, and confirm the cup method before comparing a seconds value with mPa·s.

Candidates by material interface
GradeStated referenceIntended interface
LK102430±1% solids; 20±2 sMetallized / holographic card primer
LK102525±1% solids; 20±2 sAluminum foil and foil-laminated paper
LK1026≥42% solids; 800–1500 mPa·sMetallized film, foil and barrier laminate bond
LK1029≥38% solids; peel ≥1.5 N/15 mmMetallized transfer-film coating
LK1045Approved top varnish pairing requiredUV offset drip-off / reverse-effect underlayer

How is UV drip-off contrast developed on metallized board?

LK1045 is a UV offset underlayer for matte or textured contrast against gloss areas on coated, white, metallized or holographic board. It must be paired with an approved top varnish. The reference data do not specify a universal coat weight, lamp dose or single-pass guarantee; validate the complete press and curing sequence.

Use a marked design containing fine lines, solid areas and the intended unprinted metallic regions. Compare contrast, registration and adhesion after curing and after downstream creasing. Record the actual ink, primer, top varnish and lamp configuration so a later substrate change can be evaluated against the same reference.

What should be checked when the metallic layer dulls or separates?

Separate optical change at the coated face from failure inside the laminate. LK1026 is described as non-corrosive to the aluminum layer, while LK1024 targets wetting and adhesion on decorative card. Those descriptions do not establish compatibility with every surface treatment; inspect the actual construction after the agreed conditioning and aging sequence.

Photograph the same area before coating, after drying and after storage. Identify whether the transferred layer remains on the film, the paper or the adhesive. Do not diagnose aluminum corrosion from appearance alone. Request grade-specific evidence for the exposed metal, pretreatment and contact conditions before adopting a production remedy.

What information makes a metallic-substrate trial reproducible?

Provide the layer order, exposed metallic or protective surface, application method and required appearance or peel result. For LK1029, the stated peel reference is at least 1.5 N/15 mm; request the method and test conditions. Include current TDS/SDS requirements and the exact roll or board used in the comparison.

  • Identify transferred metallization, foil lamination or holographic film.
  • Give the coater or UV offset setup and drying/curing arrangement.
  • State whether gloss, contrast, adhesion, foil appearance or peel is the acceptance criterion.