Which film and paper faces must I identify before lamination?
Record the film grade, treated face, printed paper surface and the order of every layer reaching the nip. M-7273, M-7285 and M-7298 cover PP/BOPP film-to-paper applications, while LK1038 lists paper-to-PET/PE use. Confirm the grade’s wet-bond or dry-bond route in the current TDS rather than treating these substrates as interchangeable.
Biaxially oriented polypropylene (BOPP) film can have different surfaces on its two sides. Read the roll label and record which face received adhesive. Note any primer, print, powder or varnish on the paper. Sketch the layer order and mark where the layers separated. A dyne test can screen the film for changes in wetting. The peel comparison on the finished sheet shows how the complete joint behaves.
Identify the laminating route when selecting a water-based film-to-paper lamination adhesive. A wet-bond line joins the layers while the adhesive is still wet, so the construction needs a route for water to leave. A dry-bond line dries the applied layer before the nip. Confirm which route the grade supports and record the actual dryer and nip setup before comparing rolls.
What should I check when film peels cleanly or bubbles after creasing?
Inspect where separation occurs and whether it follows the print, web width or crease. Clean film release calls for checking the treated face and coverage; ink carried away with film calls for inspecting the print interface. Bubbles need matched samples before and after conversion, with conditioning and line settings recorded.
- The film peels clean across the entire sheet. Verify roll orientation and coating continuity on a retained piece. Trial a known-good film roll on the same printed stock with the adhesive and settings unchanged.
- Only solid print areas lift. Peel an adjacent unprinted margin and a heavily inked area of the same sheet. If the ink transfers with the film and leaves exposed stock, investigate the print-to-paper interface and print drying with the printer.
- Bubbles appear in bands or only after creasing. Mark their positions relative to the web edges and the creases. Compare sheets before and after conversion. Repeating bands justify a check of adhesive coverage and nip contact across the width. A crease-localised defect calls for testing the actual crease after the recommended conditioning interval.
How should I compare peel strength without mixing test methods?
Use equal-width strips, the same peel angle and rate, and the same conditioning interval, then record force units and failure location. M-7273–M-7298 list a 48 h cure reference. LK1029’s separate ≥1.5 N/15 mm transfer-peel benchmark belongs to transfer-film coating; it must not become an assumed BOPP lamination acceptance limit.
- Retain left, centre and right samples from the same run. Label film lot, paper lot, print area, adhesive, coating weight, line speed and elapsed time before testing.
- Cut equal-width strips. Peel each in the same direction at the same angle and rate. Record width and force units for an instrumented test. Keep photographs and failure locations with each reading. A paper split measures the behaviour of the laminate at that spot and limits what the reading tells you about the adhesive interface.
- Change one suspected factor and repeat the same checks alongside the reference. Approve the job against the agreed peel result, surface appearance and behaviour after the actual fold, crease or embossing operation.
Product values are typical ranges from the supplied specifications. Use the latest grade-specific TDS/SDS and documented substrate trials for production approval. A stated benchmark is not a result measured on your construction.