LeadChem Technical enquiry

Printing

Choosing water-based ink for film and labels

Start with the print face and the end use. An exposed label has to withstand handling. An image reverse-printed inside a laminate has to stay bonded when the structure is peeled.

What film and press details are needed to select a water-based ink?

Specify the polymer, treated print face, gravure or flexo process, and whether the image remains exposed or enters a laminate. LK1035 lists corona-treated BOPP, PET and paper; LK1036 also lists PVC film. Record roll identity, metering, drying and line speed so that the candidate and existing ink can be compared.

Give the film type, treated or coated face, roll lot and whether the image will be exposed or laminated. BOPP (biaxially oriented polypropylene) and PET (polyester) are different substrates. A trial on a paper label also leaves an important question open: how will this ink dry on a non-absorbent film?

For flexographic printing, record the anilox specification and plate used for the trial. For gravure, record the cylinder and cell specification. In both cases, record line speed, dryer settings, ink temperature, pH and viscosity using the supplier's stated method. These details allow a second run to reproduce the first.

How do I separate poor wetting from drying or adhesion failure?

Check whether the defect begins while the ink is wet, during a controlled adhesion test, or after lamination. Wet ink pulling back suggests a wetting comparison; a dry print lifting needs a consistent adhesion check. LK1035 and LK1036 specify pH 8.0–9.0, but pH alone does not prove film adhesion.

What you seeFirst comparison to make
Wet ink draws back into islandsCheck the print face and compare its wetting with an approved roll. Take readings on the same side using the same method and timing. A dyne reading helps investigate wetting. It cannot establish the final bond.
A solid looks even but lifts on tapeKeep the tape, pressure and removal method constant. Compare prints after the same drying and conditioning interval. Mark whether ink releases from the film or splits within the ink layer.
The print passes handling but the laminate separatesPrepare printed and unprinted bond areas on the same film. Peel them after the agreed conditioning time and inspect both faces for transferred ink or adhesive.

Which control makes a film-ink trial interpretable?

Run the candidate and current ink on the same identified roll, artwork and press setup, then compare them after the same drying and conditioning interval. If both fail, repeat the control on an approved roll. For LK1028, confirm the viscosity cup and temperature before interpreting its supplied 25–35 s range.

Compare the candidate and current ink on the same roll with the same image, metering and drying settings. Label the print direction and treated side. If both inks fail on that roll, repeat the control on a known-good roll before altering the ink. For a surface-printed label, include the handling or rub check specified by the buyer.

Which grade should enter the trial?

For gravure, compare LK1035 white ink at 20–30 s Tu-4 and LK1036 blue ink at 18–28 s Tu-4, both at 25°C. For flexo, LK1028 lists solids ≥40% and pH 7.5–8.5. These are selection references; confirm the exact film treatment, color target, end use and current TDS before sampling.

For gravure, LK1035 is a white ink and LK1036 is a blue ink. For flexo, LK1028 is a colour ink. Identify your process, colour target and exact stock when requesting a sample. Confirm the chosen grade for the particular film, treatment and end use.

Product values are typical ranges from the supplied specifications. Use the latest grade-specific TDS/SDS and documented substrate trials for production approval. A stated benchmark is not a result measured on your construction.

Technical references