Which UV ink grades are confirmed for a mercury or LED lamp?
LK1048, LK1049, LK1052 and LK1055 are listed for mercury UV curing; LED-UV suitability must be verified by grade. Obtain confirmation for the exact color and lamp wavelength before trialing an LED press. A shared UV label, or a cured-looking surface, is not evidence that the complete ink film received sufficient exposure.
A mercury lamp emits across a broader range of wavelengths. An LED array concentrates its output in a narrow band. The photoinitiator in the ink must absorb enough light in that band to start polymerisation. Ask for the LED head’s peak wavelength in nanometres and the ink manufacturer’s supported curing systems for that grade and colour.
What exposure data should I record during a UV curing trial?
Record lamp type and wavelength, peak irradiance, dose, line speed, lamp distance and the measuring instrument. Include ink deposit, white layers and dense overprints. The supplied LK1048–LK1056 data does not establish a universal UV dose or LED wavelength, so use the grade-specific guidance and test the actual printed build.
Peak irradiance is the highest power per unit area that the print receives during a pass. Dose is the energy accumulated over the pass. Moving the sheet faster shortens its exposure at a given lamp setting. Record both readings using a radiometer suitable for the source and wavelength, together with the meter model, line speed and lamp-to-sheet distance.
Record the ink deposit and any overprint varnish as well. Pigments and thicker films can reduce the light reaching the lower part of an ink layer. Include a heavy solid, dense overprint or white ink where the artwork calls for one. Check cure on those printed areas even when the clear coating has passed.
What does a successful UV curing trial actually approve?
It approves the documented grade, color build, substrate and lamp setup against the agreed cure, adhesion, rub and converting checks. LK1040’s supplied 5B adhesion result does not establish LED compatibility or transfer to other inks. Keep the accepted sheet and exposure record, and repeat qualification when the relevant material or setup changes.
- Establish a reference. Retain an accepted sheet with its ink, substrate and lamp settings. If moving a job to LED, use the supplier-approved candidate for the new source and keep the board and artwork constant.
- Test the working range. Within the approved operating range, mark samples at normal speed and the highest intended speed. Use the ink supplier’s cure assessment, then compare adhesion and rub using the agreed methods.
- Check the converted pack. Crease and fold a printed area and inspect for lifting or cracking. Use the ink supplier’s specified through-cure check for the full ink film. For a food-packaging job, request documentation for the intended use separately.
Keep the accepted sheet and radiometer record together. A different wavelength, ink grade, colour build or press setup changes the basis of the approval.
Product values are typical ranges from the supplied specifications. Use the latest grade-specific TDS/SDS and documented substrate trials for production approval. A stated benchmark is not a result measured on your construction.