What has to happen on press?
An aqueous coating needs water removal and controlled delivery conditions; a UV varnish needs a compatible curing system and verified exposure. LK1021 lists solids ≥35%, while LK1042 lists 100% solids and 1500±300 mPa·s. These different specifications guide material selection but do not define dryer settings, lamp dose or production speed.
An aqueous overprint varnish sits on top of the ink. As water leaves the wet layer, the binder forms a film. The board, underlying ink and amount of coating all affect drying. Airflow and extraction carry water away. Excessive heat in the delivery pile can soften the surface.
A UV varnish forms its film by a light-triggered chemical reaction. The varnish must suit the lamp fitted to the press. Record the light source, measured exposure, coating deposit and line speed so that the trial can be repeated.
Why should I keep an unvarnished glue-flap control?
A matched unvarnished strip helps separate adhesive-to-finish compatibility from bead placement, compression and board behavior. Compare both faces of the seam after the same conditioning interval. Folder-gluer grades such as M-6140 list UV-coated and laminated cartons, but the actual varnish, print stack and joint geometry still require a substrate trial.
Mark the seam on a flat blank and fold it once to identify both faces that will meet. The adhesive may land on bare board while the opposite flap carries varnish. A glue-flap knockout leaves the designated bond area free of varnish. If the artwork allows it, prepare blanks with and without that knockout on the same stock.
- Compare the printed panels. Run each finish over the same artwork and ink coverage with its appropriate drying or curing setup. Compare the gloss or matte appearance with the approved sample under the same lighting.
- Convert the blanks. Run them through the production crease and fold. Inspect the outside of the fold for cracking, then rub a marked solid area using the same method and load on each sample.
- Open the seam. Keep adhesive placement, compression and conditioning time constant. Photograph both faces. A patch of colour or varnish attached to the adhesive points to a different failure layer from a clean release at the glue line.
What belongs in the approval?
Approve the coating, substrate, ink, adhesive, coating boundaries and converting sequence together, with recorded appearance, crease and seam results. LK1042’s 3H pencil-hardness value and LK1044’s 1,000-rub benchmark describe different checks. Confirm each method and conditioning requirement; neither result alone establishes glue-flap adhesion or acceptance of the complete converted carton.
Identify the coating, board, ink, adhesive and coating-free areas on the signed sample. Record the rub result, appearance at the crease and seam behaviour after conditioning. If only the unvarnished seam held, retain that knockout on the production drawing. A change to the printed or bonded surface calls for another seam trial.
Product values are typical ranges from the supplied specifications. Use the latest grade-specific TDS/SDS and documented substrate trials for production approval. A stated benchmark is not a result measured on your construction.